Please contact us for a price:
Contact UsPlace of Origin : Henan, China (Mainland)
Brand Name : PEONY
Item : Submerged Arc Welding Flux
Model Number : PW-SJ501
Performance : Stable Arc,High Speed
Application : pressure vessels,Boiler,LGP Cylinder
Certification : ABS,CCS,TUV,CE
Basic : 0.5-0.8
Color : Grey
Grain Size : 0.3-2.0mm
Standard Packaging : 25kg/55lbs
Introduction
PW.SJ501 flux is a kind of titanium-aluminum acetic sintered flux, with basicity of 0.5 ~ 0.8. The granular shape is round; size 2.0 ~ 0.28mm (10-60 mesh); color grey. During application, the arc is stable and the removal of slag is easy. The welding bead is nice. The flux has strong resistance to porosity and can still perform well even if there is some rust or other oxides on the work piece. The flux can operate on DC/AC. The wires should be connected to the positive terminal when the welding machine is set to DC current.
Uses
Working with proper welding wires (EL8,EM12 and EA2) can weld the structures made of low-carbon steel and low alloy-steel such as ship, boiler, pressure vessel; the flux working with proper wires can perform very well in the situation that requires high-speed welding on the thin steel plates.
Chemical Composition of flux (%)
Chemical Composition on | SiO2+TiO2 | CaO+MgO | Al2O3+MnO | S | P |
---|---|---|---|---|---|
Guarantee Value | — | — | — | ≤0.060 | ≤0.080 |
General Result | 30 | 59 | 8.8 | 0.039 | 0.041 |
Mechanical Properties of Deposited Metal (In accordance with GB/T5293-1999)
Test Item | Rm(N/mm2) | Rel(N/mm2) | A(%) | KV2(J) | |
---|---|---|---|---|---|
0°C | |||||
EM12 | Guarantee Value | 415 ~ 550 | ≥330 | ≥22 | ≥34 |
General Result | 480 | 375 | 27 | 64 |
Note
1. The welding electrodes should be baked 1.5 hour at 300~350℃ before welding.
2. The impurities such as rust, oil stains and moisture must be cleared off of the work piece.
Welding Positions